Ultra-dispersed diamonds(UDD)

 

 

 

 

 

 

 

 

Contents of diamonds phase: not less than 97% weight

Square surface: 300 ± m²/gr.

Size of primary micro-crystals: 4 - 6 nm

Particles primary solid aggregates: 20 - 30 nm

 

Electro-chemical metal-diamond covering

Cr. – 2 - 10 time improving of cutting tool operation period and decreasing of cutting force.

Ni. – 20 time improving of machine part wear-resistance in comparison with a pure Ni. Covering.

Ag. – 1,5 - 2 time improving of wear-resistance in comparison with pure Ag. Increase of corrosion resistance.

Au. – 2 - 3 time improving of micro-hardness without changes in electro-physical and decorative properties of Au.

 

Anti-friction lubrication compositions

  • Decrease of friction by 20 - 40%.
  • Decrease of wearing by 30 - 40%.

 


 

Polymer-diamond composite materials
  • UDD effect on a polymer matrix leads to increase of wear resistance, anti-friction, preservative, physical and mechanical properties of the basic polymer.
  • High-effective diffusion composite membranes.

 

Finishing compositions
  • Finishing high-precision clean polishing to surface roughness Rz=2 - 10 nm without surface dislocation and loads, allows to obtain thickness of articles to 10 - 20 mcm.

 

Compacts (cakes)
  • Metal-cutting, boring and abrasive tools
  • Low-defect diamond films

 


UDD Production Unit

Capacity – 1 ton of explosive > 30 - 60 kg of UDD
  • Required useful space: 1.400 - 2.100 m²
  • Total space: 1 km² (if combining stages 1and 2)
  • Initial material: trotyl-heksagen 50/50

 

Stage 1 – Obtaining TNT blocks cleaning of UDD

  • Moulding or pressing of initial material m² 1000 - 2000$/ton
  • Total space: 1 km² (without combining with stage 2)
  • Useful space: 200 - 300 m² (1 floor)

 Stage 2 – Obtaining diamond brand – explosion

  • Total space (TNT storage included): 1 km² (without combining with stage 1)
  • Useful space: 200 - 300 m²

Stage 3 – Chemical cleaning of UDD

  • Space: 1.000 - 15.000 m²

 

 


There are no analogues in the world!


 

GESTFIN Ltd

Research and Technology

on enviromental Cognizance and Management

For more information about our products and projects, please contact:

information@gestfin.com

marketing@gestfin.com

management@gestfin.com

design1@gestfin.com

design2@gestfin.com

director@gestfin.com

legal@gestfin.com


RUSSIA

GESTFIN Ltd - 1952989 - Saint Petersburg - Uliza Bieloruskaya 6 Co.2

 

ITALY

GESTFIN Ltd - Viale della Vittoria 31 - 04019 Terracina (LT)

 

RETURN TO MAIN PAGE


Copyrigth © 2001 GESTFIN Ltd

Last update 15/01/2001

For information about this site, please contact webmaster@gestfin.com